  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP21TPND-NV Two component, paste-like epoxy polysulfide
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • One to one mix ratio
  • Superior resistance to fuels and oils
  • Thixotropic paste
  • Room temperature curing compound
  • Withstands 1,000 hours 85°C/85% RH
  • Fully complies with RoHS regulations
Product Description: Master Bond EP21TPND-NV is a two component epoxy polysulfide system with a paste consistency that cures at room temperature or more rapidly at elevated temperatures. It has a forgiving one to one mix ratio by weight or volume and can be used as an adhesive, coating and sealant. It’s very resistant to a number of chemicals including water, gasoline, fuels, oils, hydrocarbons, hydraulic fluids and many acids and bases. Significantly, unlike many chemical resistant epoxy based materials, this system has excellent toughness and flexibility. The combination of properties enables EP21TPND-NV to withstand rigorous thermal cycling as well as mechanical and thermal shocks. It bonds well to a variety of substrates, including metals, glass, ceramics and many rubber and plastic materials. The cured system has excellent electrical insulation properties. Its service temperature range is -80°F to +250°F. One unusual feature of EP21TPND-NV is the influence of adding heat to the curing cycle. When cured at room temperature the Shore D hardness is 60-65 and when cured at 200°F for 2-3 hours, its hardness is 15-20 Shore D. Therefore, to optimize properties, especially its chemical resistance profile, room temperature curing only is recommended. The color of Part A is black and Part B is amber, although, other colors are available. Polysulfide based systems, including EP21TPND-NV, have been used as fuel tank sealants and as sealing compounds for electrical connectors exposed to fuels, oils and lubricants, for many years. EP21TPND-NV is also widely used in the aerospace, OEM, electronic, electrical, chemical and related industries.

Product Advantages:

  • Easy mixing, forgiving 1:1 mix ratio, weight or volume
  • Smooth paste consistency, simple to apply
  • Ambient temperature curing imparts optimal chemical resistance and hardness
  • Forms tough bonds; resistant to thermal cycling
  • Bonds well to a variety of substrates
  • Superb resistance to oils, fuels and related chemicals

Information provided by Master Bond.

Vendors:
Available Properties
  • Viscosity, Part A
  • Hardness, Shore D
  • Hardness, Shore D, after 1,000 hours 85°C/85% RH
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap shear, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Working Life, after mixing, 100 gram batch
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.