MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
SABIC VALOX™ FR 310SE0 PBT (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Specific Gravity, ASTM D792
  • Density, ISO 1183
  • Moisture Absorption, ISO 62, 23°C / 50% RH
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, SABIC method, 0.75-2.3 mm
  • Linear Mold Shrinkage, Flow, SABIC method, on Tensile Bar
  • Linear Mold Shrinkage, Flow, SABIC method, 2.3-4.6 mm
  • Linear Mold Shrinkage, Flow, SABIC method
  • Linear Mold Shrinkage, Transverse, SABIC method, on Tensile Bar
  • Linear Mold Shrinkage, Transverse, SABIC method
  • Linear Mold Shrinkage, Transverse, SABIC method
  • Melt Flow, ISO 1133, MVR, cm^3/10 min
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ISO 2039-2
  • Hardness, H358/30, ISO 2039-1
  • Tensile Strength at Break, ISO 527, 50 mm/min
  • Tensile Strength at Break, ASTM D638, 50 mm/min
  • Tensile Strength at Break, ASTM D638, Type I, 50. mm/min
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, Type I, 50 mm/min
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Break, ASTM D638, Type I, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Break, ASTM D638, Type I, 50 mm/min
  • Elongation at Yield, ISO 527, 50 mm/min
  • Elongation at Yield, ASTM D638, Type I, 50 mm/min
  • Elongation at Yield, ISO 527, 50 mm/min
  • Elongation at Yield, ASTM D638, Type I, 50 mm/min
  • Flexural Yield Strength, ISO 178, 2 mm/min
  • Flexural Yield Strength, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*4
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*4
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*4 sp=62mm
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*4 sp=62mm
  • Charpy Impact, Notched, ISO 179/2C
  • Charpy Impact, Notched, ISO 179/2C
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Instrumented Impact Total Energy, ASTM D3763
  • Taber Abrasion, mg/1000 Cycles, SABIC method, CS-17, 1 kg
  • Tangent Modulus, ISO 527, 1 mm/min
  • Tangent Modulus, ASTM D638, 5 mm/min
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093, ROA
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1, in oil
  • Dielectric Strength, IEC 60243-1, in oil
  • Dielectric Strength, IEC 60243-1, short time
  • Dielectric Strength, ASTM D149, in air
  • Dielectric Strength, ASTM D149, in oil
  • Dielectric Strength, IEC 60243-1, in oil
  • Dielectric Strength, ASTM D149, in oil
  • Dielectric Strength, IEC 60243-1, in oil
  • Dielectric Strength, IEC 60243-1, in oil
  • Dielectric Strength, IEC 60243-1, in oil
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Arc Resistance, ASTM D495
  • Arc Resistance, UL 746A
  • Comparative Tracking Index, IEC 60112
  • Comparative Tracking Index, IEC 60112
  • Comparative Tracking Index, UL 746A
  • Hot Wire Ignition, HWI, UL 746A
  • High Amp Arc Ignition, HAI, UL 746A
  • High Voltage Arc-Tracking Rate, HVTR, UL 746A
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Parallel to Flow, ASTM E 831
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Parallel to Flow, ASTM E 831
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ASTM E 831
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Thermal Conductivity, ISO 8302
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Be, Edgew 120*10*4 sp=100mm
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Be, Edgew 120*10*4 sp=100mm
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Ae, Edgew 120*10*4 sp=100mm
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ISO 306, Rate B/120
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/120
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/50
  • Vicat Softening Point, ISO 306, Rate A/50
  • UL RTI, Electrical, UL 746B
  • UL RTI, Mechanical with Impact, UL 746B
  • UL RTI, Mechanical without Impact, UL 746B
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Oxygen Index, ISO 4589
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Nozzle Temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Dry Time, Cumulative
  • Moisture Content
  • Back Pressure
  • Shot Size
  • Vent Depth
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.