CAPILENE® CT 80 A is a specialty polypropylene combining typical advantages of polypropylene random and heterophasic copolymers. Features: Excellent impact, Very low stress whitening, Mold release, Good organoleptic properties, Excellent transparency, High gloss, Clarified, Short cycle time
Uses: Thin wall packaging, Large storage boxes, Clear pails, Food packaging, Heavy duty toolboxes, Caps and closures, Toys, Containers. Processing Methods: Injection molding.Information provided by Carmel Olefins Ltd. |