Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPOM, Polyoxymethylene