Key Attributes: Abrasion Resistant; Heat Stabilized; High Flow; High Friction; High Temperature Strength; Low Shrinkage
Applications: Automotive Applications; Automotive Under the Hood; Engineering Parts; Gears; Industrial Applications; Power/Other Tools
The value listed as Molding Shrinkage ISO 294-4, was tested in accordance with S.O.P. methods.
Injection Notes: Pre-drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried.
Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 15%, and only regrind of optimum quality should be used. In any case, part properties should be checked.
Data for dry samples unless noted.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide