Available Properties |
---|
- Density, Average value: 1.05 g/cc Grade Count:467
- Water Absorption, Average value: 0.0922 % Grade Count:92
- Moisture Absorption at Equilibrium, Average value: 0.0957 % Grade Count:42
- Water Absorption at Saturation, Average value: 0.100 % Grade Count:31
- Particle Size, Average value: 1240 µm Grade Count:23
- Maximum Moisture Content, Average value: 0.0100 Grade Count:8
- Linear Mold Shrinkage, Average value: 0.00597 cm/cm Grade Count:273
- Linear Mold Shrinkage, Transverse, Average value: 0.00467 cm/cm Grade Count:3
- Melt Flow, Average value: 7.88 g/10 min Grade Count:522
- Spiral Flow, Average value: 44.5 cm Grade Count:2
- Hardness, Rockwell L, Average value: 58.9 Grade Count:69
- Hardness, Rockwell M, Average value: 66.6 Grade Count:41
- Hardness, Rockwell R, Average value: 94.3 Grade Count:81
- Ball Indentation Hardness, Average value: 79.5 MPa Grade Count:28
- Tensile Strength, Ultimate, Average value: 27.2 MPa Grade Count:273
- Tensile Strength, Yield, Average value: 25.8 MPa Grade Count:388
- Elongation at Break, Average value: 45.0 % Grade Count:447
- Elongation at Yield, Average value: 15.4 % Grade Count:86
- Modulus of Elasticity, Average value: 1.98 GPa Grade Count:295
- Flexural Yield Strength, Average value: 46.1 MPa Grade Count:338
- Flexural Modulus, Average value: 2.13 GPa Grade Count:383
- Izod Impact, Notched, Average value: 1.14 J/cm Grade Count:401
- Izod Impact, Notched, Average value: 0.537 J/cm Grade Count:16
- Izod Impact, Notched, Average value: 0.537 J/cm Grade Count:10
- Izod Impact, Notched, Average value: 0.537 J/cm Grade Count:10
- Izod Impact, Unnotched, Average value: 4.13 J/cm Grade Count:25
- Izod Impact, Notched (ISO), Average value: 8.35 kJ/m² Grade Count:74
- Izod Impact, Notched (ISO), Average value: 5.50 kJ/m² Grade Count:2
- Izod Impact, Notched (ISO), Average value: 5.50 kJ/m² Grade Count:8
- Izod Impact, Notched (ISO), Average value: 5.50 kJ/m² Grade Count:8
- Izod Impact, Unnotched (ISO), Average value: 35.8 kJ/m² Grade Count:33
- Charpy Impact Unnotched, Average value: 7.65 J/cm² Grade Count:83
- Charpy Impact Unnotched, Average value: 8.55 J/cm² Grade Count:40
- Charpy Impact, Notched, Average value: 0.970 J/cm² Grade Count:88
- Charpy Impact, Notched, Average value: 0.422 J/cm² Grade Count:12
- Gardner Impact, Average value: 22.0 J Grade Count:19
- Dart Drop, Total Energy, Average value: 14.3 J Grade Count:5
- Falling Dart Impact, Average value: 55.6 J Grade Count:25
- Falling Dart Impact, Average value: 529 J Grade Count:1
- Instrumented Impact Total Energy, Average value: 26.8 J Grade Count:4
- Tensile Creep Modulus, 1 hour, Average value: 2080 MPa Grade Count:5
- Tensile Creep Modulus, 1000 hours, Average value: 1630 MPa Grade Count:8
- Electrical Resistivity, Average value: 1.08e+17 ohm-cm Grade Count:109
- Surface Resistance, Average value: 3.22e+14 ohm Grade Count:93
- Static Decay, Average value: 0.362 sec Grade Count:6
- Dielectric Constant, Average value: 2.46 Grade Count:101
- Dielectric Strength, Average value: 48.7 kV/mm Grade Count:121
- Dissipation Factor, Average value: 0.000365 Grade Count:54
- Arc Resistance, Average value: 119 sec Grade Count:16
- Comparative Tracking Index, Average value: 454 V Grade Count:55
- Hot Wire Ignition, HWI, Average value: 20.0 sec Grade Count:14
- High Amp Arc Ignition, HAI, Average value: 112 arcs Grade Count:14
- High Voltage Arc-Tracking Rate, HVTR, Average value: 37.1 mm/min Grade Count:13
- CTE, linear, Average value: 80.3 µm/m-°C Grade Count:134
- Specific Heat Capacity, Average value: 2.06 J/g-°C Grade Count:5
- Thermal Conductivity, Average value: 0.169 W/m-K Grade Count:27
- Maximum Service Temperature, Air, Average value: 106 °C Grade Count:17
- Hot Ball Pressure Test, Average value: 78.3 °C Grade Count:3
- Deflection Temperature at 0.46 MPa (66 psi), Average value: 86.9 °C Grade Count:124
- Deflection Temperature at 1.8 MPa (264 psi), Average value: 81.8 °C Grade Count:378
- Vicat Softening Point, Average value: 95.4 °C Grade Count:435
- Heat Distortion Temperature, Average value: 87.0 °C Grade Count:11
- UL RTI, Electrical, Average value: 50.0 °C Grade Count:8
- UL RTI, Mechanical with Impact, Average value: 50.0 °C Grade Count:8
- UL RTI, Mechanical without Impact, Average value: 50.0 °C Grade Count:8
- Flammability, UL94, Grade Count:311
- Flame Spread, Average value: 29.3 mm/min Grade Count:6
- Oxygen Index, Average value: 18.0 % Grade Count:19
- Glow Wire Test, Average value: 707 °C Grade Count:19
- Haze, Average value: 5.47 % Grade Count:12
- Gloss, Average value: 67.4 % Grade Count:103
- Transmission, Visible, Average value: 86.6 % Grade Count:11
- Processing Temperature, Average value: 210 °C Grade Count:39
- Nozzle Temperature, Average value: 219 °C Grade Count:20
- Die Temperature, Average value: 217 °C Grade Count:3
- Melt Temperature, Average value: 216 °C Grade Count:178
- Mold Temperature, Average value: 49.2 °C Grade Count:149
- Injection Velocity, Average value: 200 mm/sec Grade Count:10
- Drying Temperature, Average value: 77.7 °C Grade Count:55
- Moisture Content, Average value: 0.201 % Grade Count:10
- Injection Pressure, Average value: 77.7 MPa Grade Count:11
|
| | |