Butene Copolymer Features: - Excellent processability, cold temperature impact resistance and ESCR properties
- Outstanding flexibility and warpage resistance
- Good organoleptic properties and natural color
- High surface gloss
Additives: Applications: - Thin wall lids for frozen food packaging (ice cream, whipped dairy)
- Caps and closures, tamper evident, dairy applications
- Compounding
United States: SCLAIR 2114 resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.1a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking. NOVA Chemicals polyethylene resins are biologically and chemically inert. Information provided by NOVA Chemicals® |