MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Blue River Coatings Hyfro-Flex II PIR (Heat Reflective) Polyurethane Top Coat
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: BLUE RIVER COATINGS HYDRO-FLEX II PIR POLYURETHANE TOPCOAT is a high performance, heat reflective, single component water dispersible polyurethane. HYDRO-FLEX II PIR is formulated with heat reflective pigments and adhesion promoting additives to provide the option of painting vinyl and plastic substrates with dark colors that minimize heat gain. The product provides outstanding coverage, excellent durability and is easy to apply. HYDRO-FLEX II PIR is a low VOC and EPA compliant coating.

Enviromental Advantages:BLUE RIVER COATINGS HYDRO-FLEX II PIR POLYURETHANE TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated, dried and sent to a “Class B” landfill. Check with local and state agencies for proper handling and disposal.

Characteristics:

  • Excellent adhesion on most plastic substrates to include vinyl, PVC and fiberglass
  • Excellent exterior durability
  • Excellent heat reflective properties
  • Excellent hardness/impact resistance
  • Excellent mar and abrasion resistance
  • Excellent linear flexibility
  • Non-photochemically reactive
  • Full gloss-80-85% at 60° glossometer
  • Available in satin to gloss finish
  • Coatings can be applied in a wide range of temperature and humidity without the use of retarders
  • Water is used for reduction
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • No discoloration or loss of flexibility when oven baked (250°F for one hour)
  • Wide range of colors to include metallics
  • Shelf life of 1 year
  • Single component product-unused paint can be returned to container
  • Non-Flammable

    Uses

  • Fiberglass
  • Metal
  • Rigid Vinyl
  • Most Plastics
  • Wood
  • PVC
  • Foam or Cellular PVC
  • Information provided by Blue River Coatings

    Vendors:
    Available Properties
    • Specific Gravity
    • Density
    • Solids Content, by volume
    • Solids Content, by weight
    • Volatile Organic Compounds (VOC) Content
    • Impact Test, Forward and Reverse
    • Taber Abrasion, mg/1000 Cycles, CS17 wheel, 1000 g load
    • Boiling Point
    • Flash Point
    • Cure Time, Recoat, at 50% humidity
    • Cure Time, Dust Free, at 50% humidity
    • Cure Time, Dry to handle, at 50% humidity and 75°C
    • Shelf Life
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.