Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax CA1110/1GC BLK P23444 medium high melt flow, 1,100 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a very good combination of properties and processability. It is typically used for painted automotive bumper fascia applications. Applications: Bumpers, Exterior Automotive Applications |