Tecnoflon® N 935 is a medium high viscosity fluoroelastomer copolymer. Tecnoflon® N 935 is intended as a general purpose fluoroelastomer. It can be blended with other polymers of the Tecnoflon® family to meet specific requirements. Tecnoflon® N 935 does not contain curatives: therefore the proper levels of Tecnoflon® FOR M1 and Tecnoflon® FOR M2 must be added to achieve the required properties. It can be also cured with diamine based systems such as Tecnoflon® Tecnocin A and Tecnoflon® Tecnocin B. Copolymer; General Purpose; Good Flow; Good Mold Release; Low Compression Set; Medium-high Viscosity Uses: Belts/Belt Repair; Blending; Gaskets; General Purpose; Hose; Profiles; Seals; Sheet Processing: Calendering; Compounding; Compression Molding; Extrusion Agency Ratings: FDA 21 CFR 177.2600 Availability: Europe; North America Information provided by Solvay Specialty Polymers. |