MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
ChenGuang HGA-50 Two Component Silicone Rubber for Baby Nipple
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Molecule Formula: [Si(CH3)3O]n[Si(CH3)(CH=CH2)O]m

Properties:

  • Colorless, odorless, non-toxic, non-impurity material.
  • Mixing with reinforcer, structure controller and curing agent etc, it could be made into various kinds of articles by normal processing methods.
  • Excellent insulation property.
  • Good electric arc resistance, corona resistance and electric spark resistance.
  • Good water-proof, moisture-proof, unti-impact and unti-vibration properties.
  • Good physiological inertia and good air permeation property.
Applications: It suitable to be used in the fields of aviation, navigation, instrument and meter, electronic equipment, metallurgical, mechanics, automobile industries and medical purpose etc. It can be made into sealing rings, gaskets, tubes, cables, as well as human being organs, baby nipples, blood vessel, air permeable films, rubber mould and release agent of the precision mould casting.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors:
Available Properties
  • Hardness, Shore A, JIS K6301
  • Tensile Strength at Break, JIS K6301
  • Elongation at Break, JIS K6301
  • Tear Strength, JIS K6301 (B)
  • Tensile Set, JIS K6301
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.