MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
SABIC NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes: Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimensional stability and high flow, this resin also uses non-chlorinated, non-brominated FR additives with a specific density of 1.1 g/cm^3. Noryl RN0712 may be an excellent material candidate for flat panel TV enclosure applications requiring good rheological properties, heat resistance, hydrolysis resistance and low density.

Vendors:
Available Properties
  • Density, ISO 1183
  • Viscosity, ISO 11443, Melt Viscosity, 280°C, 1500 sec-1
  • Linear Mold Shrinkage, Flow, SABIC Method
  • Melt Index of Compound, ISO 1133, MVR [cm^3/10 min]
  • Melt Index of Compound, ISO 1133, MVR [cm^3/10 min]
  • Tensile Strength at Break, ISO 527, 50 mm/min
  • Tensile Strength at Break, ASTM D638, Type I, 50 mm/min
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, Type I, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Break, SABIC - Japan Method
  • Elongation at Yield, ISO 527, 50 mm/min
  • Elongation at Yield, ASTM D638, Type I, 50 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Tensile Modulus, ASTM D638, 50 mm/min
  • Flexural Strength, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Yield Strength, ISO 178, 2 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*4 sp=62mm
  • Volume Resistivity, ASTM D257
  • Volume Resistivity, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, UL 746A
  • CTE, linear, Parallel to Flow, ASTM E 831
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ASTM E 831
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/120
  • Flammability, UL94, UL 94
  • Oxygen Index, ISO 4589
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.