MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Chemours Teflon™ NXT 85 Modified Granular PTFE Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Teflon™ PTFE NXT 85 is a free-flowing, pelletized, chemically modified granular resin (its equivalent fine-cut resin is Teflon™ NXT 75). It provides superior processing characteristics in addition to properties of chemically modified resins. When properly processed, it offers an excellent combination of properties that are characteristic of Teflon™ fluoroplastic resins. This chemically modified resin offers improved resistance to deformation under load, increased resistance to permeation of chemicals, and higher dielectric breakdown strength. Teflon™ PTFE NXT 85 provides a high degree of weldability for applications where the use of elevated temperature and pressure are limited. Teflon™ PTFE NXT 85 can be converted to parts by isostatic, billet, and sheet molding methods, as well as ram extrusion. It can be used for: Valve seats, Fittings, Pipe valve and vessel liners, Seal rings, Bearing pad, Electrical insulation. This resin is particularly useful in applications where welding of parts to other fluoropolymers such as PFA or standard PTFE is required, e.g., fluid handling systems.

Information provided by Chemours.

Vendors:
Available Properties
  • Specific Gravity, ASTM D4894
  • Bulk Density, ASTM D4894
  • Water Absorption, ASTM D570
  • Particle Size, ASTM D4894, Average
  • Deformation, ASTM D621 Method A, 24 hours
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D4894
  • Elongation at Break, ASTM D4894
  • Flexural Modulus, ASTM D790
  • Flex Crack Resistance, ASTM D2176, Cycles MIT Folding Endurance
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, ASTM D1894
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • Melting Point, ASTM D3418
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.