MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Borealis NAV101M LDPE, post-consumer recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: NAV101M is a transparent low density post-consumer recycled (rLDPE) supplied in pellet form for high-end blown film applications. NAV101M is an ideal LDPE used where sustainability and circularity matter. NAV101M is 100 % post-consumer recycled including a majority of pre-sorted municipal (household) waste. NAV101M is part of the EuCertPlast certificate according to the European Standard EN 15343:2007 (certificate available upon request). Due to the nature of recycleds, some variation in color and other product properties can be observed between batches. Cas No. 9002-88-4

Typical characteristics:

  • High transparency
  • Pellet shape: lenticular
  • Low odor
  • Filtration 100 µm
  • Available in homogenized 24-ton truckloads
Applications:
  • Collation shrink film
  • Shrink film
  • Lamination films for non food contact primary packaging
  • Non food contact primary packaging
  • Secondary and tertiary packaging where transparency is key parameter
Note: Minor quantity of BorShape" LLDPE significantly boosts mechanical performances of NAV101 helping convertors, brand owners and retailers meeting their sustainability goals without compromising key mechanical properties for similar packaging performance.

Information provided by Borealis AG

Vendors:
Available Properties
  • Bulk Density, ISO 60
  • Density, ISO 1183
  • Melt Flow, ISO 1133-1
  • Storage Temperature
  • Film Elongation at Break, MD, 527-3
  • Film Elongation at Break, TD, 527-3
  • Tensile Modulus, ISO 527-3, MD
  • Tensile Modulus, ISO 527-3, TD
  • Elmendorf Tear Strength MD, ISO 6383-2
  • Elmendorf Tear Strength TD, ISO 6383-2
  • Dart Drop Test, ISO 7765-1
  • Film Tensile Strength at Break, MD, 527-3
  • Film Tensile Strength at Break, TD, 527-3
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 45°
  • Melt Temperature
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.