Adstif from LyondellBasell is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability. Adstif HA849K is a very high stiffness and high clarity polypropylene homopolymer with very high stiffness, low odor transfer, very high heat resistance. Typical customer applications include thermoformed food containers, high barrier packaging, microwavable packaging that are hot fillable and microwavable with good top load strength. |