MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
SABIC Lexan® HPS1S PC  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains a higher amount of mold release than HPS1R.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ASTM D792
  • Density, ISO 1183
  • Moisture Absorption, ISO 62, 23°C / 50% RH
  • Moisture Absorption at Equilibrium, ASTM D570
  • Moisture Absorption at Equilibrium, ASTM D570
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, SABIC Method
  • Melt Flow, ASTM D1238
  • Melt Index of Compound, ISO 1133, MVR [cm^3/10 min]
  • Hardness, Rockwell M, ASTM D785
  • Hardness, Rockwell R, ASTM D785
  • Hardness, H358/30, ISO 2039-1
  • Tensile Strength at Break, ISO 527, 50 mm/min
  • Tensile Strength at Break, ASTM D638, Type I, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, Type I, 50 mm/min
  • Tensile Strength, Yield, ISO 527, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Elongation at Break, ASTM D638, Type I, 50 mm/min
  • Elongation at Yield, ASTM D638, Type I, 50 mm/min
  • Elongation at Yield, ISO 527, 50 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Tensile Modulus, ASTM D638, 50 mm/min
  • Flexural Yield Strength, ISO 178, 2 mm/min
  • Flexural Yield Strength, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ISO 178, 2 mm/min
  • Izod Impact, Notched, ASTM D256, colors
  • Izod Impact, Notched, ASTM D256, natural, tints
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*3
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*3
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*3
  • Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*3
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*3 sp=62mm
  • Charpy Impact Unnotched, ISO 179/1eU, Edgew 80*10*3 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*3 sp=62mm
  • Charpy Impact, Notched, ISO 179/1eA, Edgew 80*10*3 sp=62mm
  • Tensile Impact Strength, ASTM D1822, Type S
  • Dart Drop, Total Energy, ASTM D3763, Instrumented Impact Energy @ peak
  • Dart Drop, Total Energy, ASTM D3029
  • Dart Drop, Total Energy, ASTM D3763
  • Taber Abrasion, mg/1000 Cycles, ASTM D1044, CS-17, 1 kg
  • Volume Resistivity, IEC 60093
  • Volume Resistivity, ASTM D257
  • Surface Resistance, IEC 60093, ROA
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149, in air
  • Dielectric Strength, IEC 60243-1, in oil
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, ASTM D150
  • CTE, linear, Parallel to Flow, ASTM E 831
  • CTE, linear, Parallel to Flow, ISO 11359-2
  • CTE, linear, Transverse to Flow, ASTM E 831
  • CTE, linear, Transverse to Flow, ISO 11359-2
  • Specific Heat Capacity, ASTM C351
  • Thermal Conductivity, ASTM C177
  • Thermal Conductivity, ISO 8302
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Be, Edgew 120*10*4 sp=100mm
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Ae, Edgew 120*10*4 sp=100mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/50
  • Vicat Softening Point, ISO 306, Rate B/120
  • Oxygen Index, ISO 4589
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003
  • Transmission, Visible, ASTM D1003, 2.54 mm
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.