Available Properties |
---|
- Density, ISO 1183, Method A
- Density, ISO 1183, Method A
- Water Absorption, ASTM D570
- Linear Mold Shrinkage, Flow, ASTM D955, Conditioned
- Linear Mold Shrinkage, Flow, ASTM D955
- Linear Mold Shrinkage, Transverse, ASTM D955, Conditioned
- Linear Mold Shrinkage, Transverse, ASTM D955
- Hardness, Rockwell R, ASTM D785
- Tensile Strength at Break, ISO 527-2
- Tensile Strength at Break, ISO 527-2
- Tensile Strength at Break, ISO 527-2
- Tensile Strength at Break, ISO 527-2
- Tensile Strength, ASTM D638, Conditioned
- Tensile Strength, ASTM D638
- Elongation at Break, ASTM D638, Conditioned
- Elongation at Break, ASTM D638
- Elongation at Break, ISO 527-2
- Elongation at Break, ISO 527-2
- Elongation at Break, ISO 527-2
- Elongation at Break, ISO 527-2
- Tensile Modulus, ASTM D638, Conditioned
- Tensile Modulus, ASTM D638
- Tensile Modulus, ISO 527-2
- Tensile Modulus, ISO 527-2
- Tensile Modulus, ISO 527-2
- Tensile Modulus, ISO 527-2
- Flexural Strength, ASTM D790, Conditioned
- Flexural Strength, ASTM D790
- Flexural Strength, ISO 178
- Flexural Strength, ISO 178
- Flexural Strength, ISO 178
- Flexural Strength, ISO 178
- Flexural Modulus, ASTM D790, Conditioned
- Flexural Modulus, ASTM D790
- Flexural Modulus, ISO 178
- Flexural Modulus, ISO 178
- Flexural Modulus, ISO 178
- Flexural Modulus, ISO 178
- Compressive Strength, ASTM D695
- Poissons Ratio, ASTM E132
- Shear Strength, ASTM D732, Conditioned
- Shear Strength, ASTM D732
- Izod Impact, Notched, ASTM D256, Conditioned
- Izod Impact, Notched, ASTM D256
- Izod Impact, Unnotched, ASTM D256
- Izod Impact, Notched (ISO), ISO 180, Type 1, Notch A
- Izod Impact, Unnotched (ISO), ISO 180, Type 1
- Charpy Impact Unnotched, ISO 179, Type 1, Edgewise
- Charpy Impact, Notched, ISO 179, Type 1, Edgewise, Notch A
- Volume Resistivity, ASTM D257, Conditioned
- Volume Resistivity, ASTM D257
- Dielectric Constant, ASTM D150
- Dielectric Constant, ASTM D150, Conditioned
- Dielectric Constant, ASTM D150
- Dielectric Constant, ASTM D150, Conditioned
- Dielectric Strength, ASTM D149, Conditioned
- Dielectric Strength, ASTM D149
- Dissipation Factor, ASTM D150
- Dissipation Factor, ASTM D150, Conditioned
- Dissipation Factor, ASTM D150
- Dissipation Factor, ASTM D150, Conditioned
- Arc Resistance, ASTM D495, Conditioned
- Arc Resistance, ASTM D495
- Comparative Tracking Index, UL 746, Conditioned
- Comparative Tracking Index, UL 746
- CTE, linear, Parallel to Flow, ASTM E831
- CTE, linear, Parallel to Flow, ASTM E831
- CTE, linear, Transverse to Flow, ASTM E831
- CTE, linear, Transverse to Flow, ASTM E831
- Melting Point, ASTM D3418, Peak
- Melting Point, ISO 11357-3
- Maximum Service Temperature, Air, ASTM D794, Continuous
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Annealed
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2/A, Unannealed
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
- Flammability, UL94
- Rear Barrel Temperature
- Front Barrel Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Moisture Content
|
| | |