MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
DuPont Styrofoam™ Tongue and Groove Extruded Polystyrene Foam Insulation
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: STYROFOAM™ Brand Tongue and Groove Insulation features tongue and groove edges on all four sides of 2’ x 8’ boards 1” thick or less and on the long edges of all other boards. The lightweight, moisture-resistant and thermally efficient Type IV extruded polystyrene foam insulation is suited for a wide range of residential and commercial construction applications. STYROFOAM™ Brand Tongue and Groove Extruded Polystyrene Foam Insulation (XPS) goes up quickly and easily with groves on all four edges to lock into the next sheet and gives more coverage per board. It’s easy to install with high compressive strength for above and below grade applications including:
  • Exterior walls
  • Interior walls
  • Ceiling
  • Exterior foundation walls
  • Interior foundation walls
  • Crawl space
STYROFOAM™ Brand Tongue and Groove Insulation is suitable for use in pervious, semi-pervious and practically impervious soils.

This material is produced as sheets of closed-cell foam by a continuous extrusion process. Its properties will be different than expanded polystyrene beads because beads have voids between cell walls.

This former Dow product line is now a DuPont product line.

Vendors:
Available Properties
  • Water Absorption, ASTM C272, volume%
  • Flexural Strength, ASTM C203
  • Compressive Strength, ASTM D1621
  • CTE, linear, ASTM D696
  • Insulation R Value, ASTM C518
  • Insulation R Value, ASTM C518
  • Insulation R Value, ASTM C518
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Packaging and Industrial Polymers

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.