Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposit and enhanced crystallization for low porosity.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPOM, Polyoxymethylene