Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing into solutions and to improve adhesion to substrates when used as a coating. Veradel® 3600RP r-PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water and mineral acids. Cast films or coatings of r-PESU are transparent and have additional desirable properties, including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance. Veradel® r-PESU polymers are available in two molecular weight regimes. Veradel® 3000RP is a high molecular weight sulfone polymer with a relatively low level of functionality while Veradel® 3600RP has a lower molecular weight sulfone polymer (approximately half the molecular weight of the Veradel® 3000RP) with roughly 3-5 times higher level of functionality. The differences in molecular weight results in highly varied levels of viscosity, when measured under similar conditions. Typical applications include high-temperature coating formulations and specialty adhesives. Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Flow; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Low Molecular Weight; Medium Rigidity Uses: Adhesives; Binder; Coating Applications Processing: Coating; Solution Processing; Spraying Agency Ratings: NSF STD-51 Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Information provided by Solvay Specialty Polymers. |