Typical applications include thermoformed trays and clamshells which give permanent ESD protection for the electronics, medical, pharmaceutical industries.
Information provided by Premix Thermoplastics Inc.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic