MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Redwood Plastics REDCO™ LOAD+™ Fiber reinforced rubber pads
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Overview: DYNAMEX™ LOAD+™ fiber reinforced rubber pads are structural bearings with higher stiffness (see Figure 4). They are commonly used in applications involving higher load requirements and less rotational needs. Consisting of high-strength, weather resistant elastomers and vulcanized with synthetic reinforcing fibres, our pads are designed for structural projects with typical design loads of 2000psi.

Applications: DYNAMEX™ LOAD+™ is widely used in pre-cast concrete structural applications. Examples include beams, Tees, hollow core slabs or girders in precast and prestressed concrete structures such as parking garages, pedestrian overpasses, masonry pads and many more.

Product Details: Stocked from 3/8” thickness through to 1” thickness, DYNAMEX™ LOAD+™ pads can be supplied in full sheet, strips or cut-to-size. The material can be moulded and fully fabricated to meet additional requirements. Table 5 displays the material properties for these pads.

Information provided by Redwood Plastics and Rubber

Vendors:
Available Properties
  • Density, ASTM D 297
  • Hardness, Shore A
  • Hardness, Shore A, ASTM D 2240
  • Tensile Strength, ASTM D 412, Die C
  • Tensile Strength, ASTM D 573
  • Elongation at Break, ASTM D 412, Ultimate
  • Elongation at Break, ASTM D 573, Ultimate
  • Compressive Strength, ASTM D 412
  • Tear Strength, ASTM D 624, Die B
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.