MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
LCY ValuPrene p-TPV 55A BK Thermoplastic Vulcanized Elastomers
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A medium hardness, black color, multi-purpose thermoplastic elastomer featuring good compression set and moderate temperature performance. ValuPrene 55A BK can be processed by extrusion for applications such as weatherstrip profile, seals, and window gaskets.

Attributes:

  • ValuPrene p-TPV is designed for applications requiring sealing performance at moderate temperatures.
  • Suitable for profile extrusion.
  • Conventional thermoplastic processing equipment can be used.
Applications: ValuPrene p-TPV has good sealing property, chemical, weathering resistance and electrical property that is suitable for TPV, thermoset EPDM rubber, Styrene based TPE, flexible PVC and other TPE applications. It is a good choice for applications requiring flexibility in the following markets: automotive parts, appliance, construction, consumer products, and electronics.

Information provided by LCY Chemical Corp.

Vendors:
Available Properties
  • Density, ISO 1183
  • Hardness, Shore A, ISO 868, Injection Molded
  • Tensile Strength at Break, ISO 37, 500 mm/min
  • Elongation at Break, ISO 37, 500 mm/min
  • 100% Modulus, ISO 37, 500 mm/min
  • Tear Strength, ISO 34-1, 500 mm/min
  • Compression Set, ISO 815
  • Compression Set, ISO 815
  • Melting Point
  • Zone 1, Extrusion
  • Zone 2, Extrusion
  • Zone 3, Extrusion
  • Zone 4, Extrusion
  • Zone 5, Extrusion
  • Die Temperature, Extrusion
  • Melt Temperature, Extrusion
  • Roll Temperature, Extrusion
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.