Adstif from LyondellBasell is a trade name for select polypropylene resins with high crystallinity used to produce customer applications, such as thermoformed containers, injection molded packaging and consumer goods. Adstif's property and performance characteristics include high crystallinity, broad processing window, high stiffness and good dimensional stability. Adstif HA748L is a high crystallinity polypropylene homopolymer with very good long term thermal stability, high stiffness, high HDT, good surface hardness, and good pigment dispersion. Typical customer applications are parts of electric appliances such as rice cooker, microwave oven, electric kettle, as well as food containers, housewares and base resin of compounds. |