Product Description: PP 523P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties required for the stenter film process. PP 523P is suitable for metallizable film, both as monolayer and in co-extruded structures. Films produced using PP 523P will exhibit:- Consistent processability
- Very good film profile
- Excellent optical properties
- High tensile properties
- Low residual ash
- Film produced can be metalized
Typical Applications: PP 523P can be used as core layer in co-extruded film and/or as base material for plain films used for stationary, dry food bags, synthetic paper and heat sealable packaging films. Information provided by SABIC. |