Available Properties |
---|
- Specific Gravity, ASTM D792
- Density, ISO 1183
- Water Absorption, ISO 62, 23°C/sat
- Moisture Absorption at Equilibrium, ASTM D570
- Linear Mold Shrinkage, Flow, SABIC method
- Linear Mold Shrinkage, Flow, SABIC method
- Melt Flow, ISO 1133, cm³/10 min
- Melt Flow, ASTM D1238
- Hardness, Rockwell R, ISO 2039-2
- Hardness, Rockwell R, ASTM D785
- Tensile Strength, Yield, ISO 527, 50 mm/min
- Tensile Strength, Yield, ASTM D638, 50 mm/min
- Elongation at Break, ISO 527, 50mm/min
- Elongation at Break, ASTM D638, 50mm/min
- Elongation at Yield, ISO 527, 50 mm/min
- Elongation at Yield, ASTM D638, 50 mm/min
- Tensile Modulus, ASTM D638, 50 mm/min
- Tensile Modulus, ISO 527, 1mm/min
- Flexural Yield Strength, ASTM D790, 1.3 mm/min, 50 mm span
- Flexural Yield Strength, ISO 178, 2 mm/min
- Flexural Modulus, ISO 178, 2 mm/min
- Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
- Izod Impact, Notched, ASTM D256
- Izod Impact, Unnotched, ASTM D4812
- Izod Impact, Notched (ISO), ISO 180/1A, 80*10*3
- Izod Impact, Notched (ISO), ISO 180/1A, 80*10*3
- Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*3
- Izod Impact, Unnotched (ISO), ISO 180/1U, 80*10*3
- Dart Drop, Total Energy, ASTM D3763, peak
- Volume Resistivity, IEC 60093
- Volume Resistivity, ASTM D257
- Dielectric Constant, ASTM D150
- Dielectric Constant, ASTM D150
- Dielectric Constant, IEC 60250
- Dielectric Constant, IEC 60250
- Dielectric Strength, ASTM D149
- Dielectric Strength, IEC 60243-1
- Dissipation Factor, ASTM D150
- Dissipation Factor, IEC 60250
- Dissipation Factor, ASTM D150
- Dissipation Factor, IEC 60250
- CTE, linear, Parallel to Flow, ASTM E831
- CTE, linear, Parallel to Flow, ISO 11359-2
- Thermal Conductivity, ISO 8302
- Thermal Conductivity, ASTM C177
- Hot Ball Pressure Test, IEC 60695-10-2
- Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Bf, Flatw 80*10*4 sp=64mm
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
- Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
- Vicat Softening Point, ASTM D1525, Rate B/50
- Vicat Softening Point, ISO 306, Rate B/50
- Flammability, UL94, UL 94
- Refractive Index, ASTM D542
- Refractive Index, ISO 489
- Haze, ASTM D1003
- Transmission, Visible, ASTM D1003
- Processing Temperature, Hopper Temperature
- Processing Temperature, Hopper Temperature
- Nozzle Temperature, Injection Molding
- Zone 1, Profile Extrusion
- Zone 1
- Zone 2, Profile Extrusion
- Zone 2
- Zone 3, Profile Extrusion
- Zone 3
- Zone 4, Profile Extrusion
- Adapter Temperature, Profile Extrusion
- Die Temperature, Profile Extrusion
- Melt Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature, Injection Molding
- Drying Temperature, Profile Extrusion
- Dry Time, Profile Extrusion
- Dry Time, Injection Molding
- Moisture Content
- Moisture Content
- Precipitation Temperature, Calibrator
|
| | |