Hifax polypropylene resins based on the Catalloy process from LyondellBasell are used by customers in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable) and also automotive industries through both our resins and our well-known Hifax polypropylene compounds. Hifax is proven to provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion. Hifax TYC 852P E C12716 is a 22% talc filled PP copolymer, with high flowability, high impact resistance and low CLTE. Product is available as a customized color matched, pellet form. This grade is delivered in C12716 color version. Applications: Bumpers |