MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK), Carbon Fiber + Graphite Lubricant  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the other members of the AvaSpire® AV-700 series, AV-755 SL45 offers more attractive economics than PEEK while retaining most of PEEK's key attributes. In addition to the outstanding wear resistance, the resin also offers the outstanding combination of chemical resistance, mechanical strength and stiffness at elevated temperatures, as well as long-term and high temperature thermal-oxidative stability. AV-755 SL45 is formulated with a binary anti-friction/anti-wear additive system comprised of carbon fiber and graphite. By virtue of its additive system, this resin also offers, exceptionally high stiffness and very low moisture absorption.

Potential applications for AV-755 SL45 include bushings, bearings, wear strips, wear rings, rollers, and other parts used in sliding friction components.

This high flow (low viscosity) resin is black.

Key Attributes: Chemical Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; Wear Resistant

Applications: Automotive Applications; Bearings; Bushings; Rollers; Seals; Thrust Washer; Wear Strip

Injection Notes: Back Pressure: Minimum

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Viscosity, ASTM D3835
  • Linear Mold Shrinkage, Flow, ASTM D255
  • Linear Mold Shrinkage, Transverse, ASTM D255
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, ASTM D638, 5.0 mm/min
  • Tensile Strength, Yield, ISO 527-2, Type 1A
  • Elongation at Break, ISO 527-2, Type 1A
  • Tensile Modulus, ISO 527-2, 1 mm/min; Type 1A
  • Tensile Modulus, ASTM D638, 5.0 mm/min
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Unnotched (ISO), ISO 180
  • CTE, linear, Parallel to Flow, ASTM E831
  • Specific Heat Capacity, ASTM C351
  • Specific Heat Capacity, ASTM C351
  • Thermal Conductivity, ASTM C177
  • Melting Point, ASTM D3418, Peak
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Glass Transition Temp, Tg, DSC
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.