LEXAN EFR85-701 film is a black color Eco flame-retardant polycarbonate film with a UL94 V-0 listing at 0.38 mm and VTM0 at 0.178mm. This film has formability, excellent mechanical and electrical properties, good dimensional stability at high temperatures and a high flammability rating, making it good for applications such as power supply insulation, disc drive insulation, bus-bar insulation, TV/monitor insulation, PC board insulation, and business equipment insulation and has insulation and EMI/RFI shielding when laminated with metal foil.Information provided by SABIC |