MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Kraiburg TPE THERMOLAST® K TC6AIB SEBS Natural High Performance TPE  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:
  • High performance SEBS compound
  • Easy to color adhesion to polyolefins
  • Excellent mechanical properties

Typical Applications:

  • Automotive Indoor:
    • Anti-slip mats
    • Soft touch for thumb wheel
  • Soft Touch:
    • Tracer
    • Push button
    • Switch
  • Handles:
    • Screwdriver
    • Toolbox
    • Skis poles
    • Hiking sticks
  • Design-Functional Elements:
    • Packaging

Material Advantages:

  • High qualitative standard SEBS-compounds
  • Excellent mechanical properties
  • Adhesion to polyolefins
  • Excellent flow characteristics

Processing:

  • Like polyolefins
  • High injection speed and pressure

Information provided by Kraiburg TPE.

Vendors:
Available Properties
  • Density, DIN 53479
  • Hardness, Shore A, DIN 53505
  • Tensile Strength at Break, DIN 53504
  • Elongation at Break, DIN 53504
  • Tear Strength, DIN 53515
  • Compression Set, ISO 815, 24 hours
  • Compression Set, ISO 815, 24 hours
  • Compression Set, ISO 815
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.