MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Nouryon Trigonox 21S Thermoset ROW tert-Butyl peroxy-2-ethylhexanoate
Categories: Other Engineering Material

Material Notes: Trigonox 21S is a peroxide formulation used for curing unsaturated polyester resin at elevated and high temperatures. Suitable as a kicker in formulations for pultrusion and SMC/BMC.

CAS number: 3006-82-4

EINECS/ELINCS No: 221-110-7

Applications: For polymer production: Polymerization of ethylene: Trigonox 21S is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. Polymerization of styrene: in suspension polymerization processes, Trigonox 21S can be used for the polymerization of styrene at approximately 90°C. Trigonox 21 has an activity comparable with Dibenzoyl peroxide (Perkadox L-W75). Typically, Trigonox 21S is used in combination with initiators such as tert- Butyl peroxybenzoate (Trigonox C) and tert-Butylperoxy 2 ethylhexyl carbonate (Trigonox 117). For Thermoset: Trigonox 21S, tert-butyl peroxy 2 ethylhexanoate, is a perester which is used for the curing of unsaturated polyester resin at elevated and high temperatures. Trigonox 21S is preferred for the curing of UP resin based Hot Press Moulding formulation (such as SMC and BMC) in the temperature range of 120 - 160°C. As Trigonox 21S is a high reactive peroxide, it is very suitable as a kicker in formulations for pultrusion and SMC/BMC. In combination with a cobalt accelerator, Trigonox 21S is also applicable for the cure of UP resins in the temperature range of 60°C and higher. Application area can be air drying lacquers, diplacquers, wall panels, filament winding, etc.

Information provided by Nouryon

Vendors:
Available Properties
  • Density
  • Half-life, [hr]
  • Half-life, [hr]
  • Half-life, [hr]
  • Viscosity
  • Molecular Weight
  • Storage Temperature
  • Decomposition Temperature, Self-Accelerating Decomposition Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.