Features: Ductile; Good Chemical Resistance; Heat Stabilized; Hot Water Moldability; Impact Modified; Low Temperature Impact Resistance; Low Warpage; Lubricated
Uses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Machine/Mechanical Parts; Metal Replacement; Valves/Valve Parts
Injection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.
Automotive Specifications DELPHI M-4853 Color: BK718 Black; DELPHI MS008756 Color: NT Natural; DELPHI MS008759 Color: BK718 Black; FORD WSS-M4D1008-A1; GM GMP.PPA.015 Color: Black; GM GMP.PPA.015 Color: Natural; GM GMW16799P-PPA Color: Natural; IMDS ID 11974222 Color: Black; IMDS ID 11974222 Color: Natural
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlastic