MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
HB Fuller EV Seal 500 Hot Melt PSA
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: EV Seal 500 is a thermal plastic hot melt PSA designed for use in gasketing and sealing applications. It is especially suitable for sealing battery pack modules where accessibility and serviceability are a high priority. With the resealable nature of this material, repeated opening and closing of a battery enclosure is simple, easy, and reliable. The EV Seal 500 offers a robust solution for preventing dust & moisture intrusion to any enclosure. This material is recommended for use with steel, aluminum, and cast iron.

Features and Benefits:

  • One component requires no mixing
  • Thermoplastic nature allows for ease of use
  • Excellent resistance to dust or moisture intrusion
  • Wide Service Temperature Range (-40°C to 110°C)
  • Re-sealable capabilities improve serviceability of enclosure
  • Suitable for easy processing with proper hot melt dispense systems
  • Outstanding absorption of shock, vibration, and CTE
  • End of life recyclability

Information provided by H.B. Fuller Company

Vendors:
Available Properties
  • Specific Gravity, Water Displacement
  • Brookfield Viscosity, #29; 20RPM
  • Storage Temperature
  • Tensile Strength, ASTM D412, Die C
  • Elongation at Break
  • Adhesive Bond Strength, Cross Pluck at 0.2”/min
  • Penetration, ASTM D217, [ddm], Cone, 150g added wt
  • Compression Set, 50% Compression
  • Compression Set, 50% Compression
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.