MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Go Yen Chemical Goyenchem-FRE70 Advanced Flame Retard Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Advantages:
  • Goyenchem-FRE70 with outstanding flame retardancy
  • Fabulous operation convenience
  • Wonderful dispersion ability and compatibility with various kinds of resin
  • Goyenchem-FRE70 can be directly compounding with general resin
  • Processing with flame retard elastomer can avoid dust pollution
  • Widely apply in various kinds of common resin and engineering plastic
  • Enhance the added-value of end products
  • Can help to reduce R &D cost
  • Total eco-friendly
  • Suitable for different kinds of process ex. Extrusion, injection molding or blown-film
Applications:
  • Flame retard HDPE?LDPE?LLDPE and so on
  • Can directly apply in PP?EVA?PVC?POE and other Polyolefin resin compounding
  • Nylon and other engineering plastic
  • Wires and cable flame retard master batch
  • E&E equipment flame retard
  • Various kinds of nature and synthetic rubber flame retard, such as EPDM, BR, IR, CR etc.
  • Comprehensive application elastomer for flame retard products
  • For flame retard elastomers like TPE?TPU?SBS?SEBS?TPO?TPV?TPEE
  • Other exclusion, injection molding, blown-film applications

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Softening Point
  • Brittleness Temperature, F50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.