Available Properties |
---|
- Density, ASTM D792
- Tensile Strength at Break, ASTM D638, 5 mm/min; ZX ORIENTATION
- Tensile Strength at Break, ASTM D638, 5 mm/min; XY ORIENTATION
- Tensile Strength at Break, ASTM D638, 5 mm/min; XZ ORIENTATION
- Elongation at Break, ASTM D638, 5 mm/min; ZX ORIENTATION
- Elongation at Break, ASTM D638, 5 mm/min; XZ ORIENTATION
- Elongation at Break, ASTM D638, 5 mm/min; XY ORIENTATION
- Tensile Modulus, ASTM D638, XY ORIENTATION
- Tensile Modulus, ASTM D638, ZX ORIENTATION
- Tensile Modulus, ASTM D638, XZ ORIENTATION
- Flexural Modulus, ASTM D790, 1.3 mm/min; ZX ORIENTATION
- Flexural Modulus, ASTM D790, 1.3 mm/min; XY ORIENTATION
- Flexural Modulus, ASTM D790, 1.3 mm/min; XZ ORIENTATION
- Izod Impact, Notched, ASTM D256, ZX ORIENTATION
- Izod Impact, Notched, ASTM D256, XY ORIENTATION
- Izod Impact, Notched, ASTM D256, XZ ORIENTATION
- Izod Impact, Notched, ASTM D256, ZX ORIENTATION
- Izod Impact, Notched, ASTM D256, XY ORIENTATION
- Izod Impact, Notched, ASTM D256, XZ ORIENTATION
- Izod Impact, Unnotched, ASTM D256, ZX ORIENTATION
- Izod Impact, Unnotched, ASTM D256, XY ORIENTATION
- Izod Impact, Unnotched, ASTM D256, XZ ORIENTATION
- Izod Impact, Unnotched, ASTM D256
- Izod Impact, Unnotched, ASTM D256
- Izod Impact, Unnotched, ASTM D256
- Dart Drop, Total Energy, ASTM D3763, XY ORIENTATION
- Dart Drop, Total Energy, ASTM D3763, XZ/ZX ORIENTATION
- Dart Drop, Total Energy, ASTM D3763, XZ/ZX ORIENTATION
- Dart Drop, Total Energy, ASTM D3763, XY ORIENTATION
- Volume Resistivity, ASTM D257, XY ORIENTATION
- Volume Resistivity, ASTM D257, XZ/ZX ORIENTATION
- Dielectric Constant, ASTM D150, XY ORIENTATION at 1.9 GHz
- Dielectric Constant, ASTM D150, XZ/ZX ORIENTATION at 1.9 GHz
- Dissipation Factor, ASTM D150, XY ORIENTATION
- Dissipation Factor, ASTM D150, XZ/ZX ORIENTATION
- CTE, linear, Parallel to Flow, ASTM E831, XY ORIENTATION
- CTE, linear, Parallel to Flow, ASTM E831, ZX ORIENTATION
- CTE, linear, Parallel to Flow, ASTM E831, XZ ORIENTATION
- CTE, linear, Transverse to Flow, ASTM E831, XY ORIENTATION
- CTE, linear, Transverse to Flow, ASTM E831, ZX ORIENTATION
- CTE, linear, Transverse to Flow, ASTM E831, XZ ORIENTATION
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
- Vicat Softening Point, ASTM D1525, Rate A/50; XY ORIENTATION
- Vicat Softening Point, ASTM D1525, Rate A/50; XZ ORIENTATION
- Vicat Softening Point, ASTM D1525, Rate A/50; ZX ORIENTATION
- Flammability, UL94, UL 94, ZX ORIENTATION, 3.0 mm (Black)
- Flammability, UL94, UL 94, XY ORIENTATION, 3.0 mm (White)
- Flammability, UL94, UL 94, XZ ORIENTATION, 3.0 mm (White)
- Flammability, UL94, UL 94, ZX ORIENTATION, 3.0 mm (White)
- Flammability, UL94, UL 94, XY ORIENTATION, 3.0 mm (Black)
- Flammability, UL94, UL 94, XZ ORIENTATION, 3.0 mm (Black)
|
| | |