MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Polyplastic Compounds Tehnamid® A-SV25-OD Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: 25% glass-filled flame retardant polyamide 66. It is intended for the production by injection molding of various parts and products for electrical and general purposes used in electrical engineering, electronics, lighting fixtures, fire fighting equipment, household appliances, instrument making and other industries. It can also be used for the manufacture of particularly critical parts of electrical devices with increased requirements for rigidity and heat resistance, including cases of automatic switches. Serially produced in gray and black.

Information provided by Polyplastic Compounds

Vendors:
Available Properties
  • Density, GOST 15139
  • Linear Mold Shrinkage, Flow, GOST 18616
  • Linear Mold Shrinkage, Transverse, GOST 18616
  • Melt Flow, GOST 11645
  • Tensile Strength, GOST 11262
  • Elongation at Break, GOST 11262
  • Flexural Strength, GOST 4648, at maximum load
  • Flexural Modulus, GOST 9550
  • Charpy Impact Unnotched, GOST 4647
  • Volume Resistivity, GOST 6433.2
  • Dielectric Strength, GOST 6433.3
  • Comparative Tracking Index, GOST 27570.0
  • CTE, linear, GOST 15173
  • Melting Point, GOST 21553
  • Deflection Temperature at 1.8 MPa (264 psi), GOST 12021
  • Flammability, UL94, GOST 28157
  • Glow Wire Ignition Temperature, GOST 27483
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.