MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Syensqo (Solvay Specialty Polymers) Omnix® FC-4050 High Performance Polyamide  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Omnix® FC-4050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture absorption. Omnix® FC-4050 is characterized by high stiffness and strength, very good impact properties, good dimensional stability and high flow properties. This material is an economical alternative for food service applications using die-cast alloys. Omnix® FC-4050 is cleared for food contact use by European Union and United States Food and Drug Administration (FDA) regulations. It processes readily using conventional injection molding machines and methods. Water-cooled molds are suitable for use with this grade.

Natural: Omnix® FC-4050 NT 000

Black: Omnix® FC-4050 BK 001

Availability:

  • Asia Pacific
  • Europe
  • North America
Features:
  • Fast Molding Cycle
  • Good Dimensional Stability
  • Good Impact Resistance
  • Good Surface Finish
  • High Flow
  • High Stiffness
  • High Strength
  • Hot Water Moldability
  • Paintable
Uses:
  • Appliances
  • Food Service Applications
Forms: Pellets

Processing Method:

  • Injection Molding
  • Water-Heated Mold Injection Molding

Information provided by Solvay

Vendors:
Available Properties
  • Density, ASTM D792
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Tensile Strength, Yield, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/A
  • Izod Impact, Unnotched (ISO), ISO 180/A
  • Melting Point, ISO 11357-3
  • Processing Temperature, Melt
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic
PA, Polyamide

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.