MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ 1010M PEI (Europe)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM 1010M resin is an amorphous, transparent polyetherimide (PEI) plastic offering a glass transition temperature (Tg) of 217?C. This inherently flame retardant resin is RoHS compliant. ULTEM 1010M resin is an unreinforced general purpose grade offering high heat resistance, high strength and modulus and broad chemical resistance up to high temperatures with enhanced flow and optimized mold release for metallized reflectors.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Moisture Absorption 0.700 %0.700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.25 %1.25 %ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inon Tensile Bar; SABIC method
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 340 °C
13 g/10 min
@Load 11.0 lb,
Temperature 644 °F
MVR, cm^3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, H358/30 140 MPa20300 psiISO 2039-1
Tensile Strength at Break 85.0 MPa12300 psi50 mm/min; ISO 527
Tensile Strength, Yield 105 MPa15200 psi50 mm/min; ISO 527
Elongation at Break 60 %60 %50 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527
Flexural Yield Strength 160 MPa23200 psi2 mm/min; ISO 178
Flexural Modulus 3.30 GPa479 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Taber Abrasion, mg/1000 Cycles 1010CS-17, 1 kg; SABIC method
Tangent Modulus 3300 MPa479000 psi1 mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
@Thickness 1.60 mm
711 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
Dissipation Factor  0.00050
@Frequency 50.0 - 60.0 Hz
0.00050
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0025
@Frequency 2.45e+9 Hz
0.0025
@Frequency 2.45e+9 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 V100 VIEC 60112
 150 V150 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 195 °C383 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 211 °C412 °FRate B/50; ISO 306
 212 °C414 °FRate B/120; ISO 306
 215 °C419 °FRate A/50; ISO 306
Flammability, UL94  V-0
@Thickness 0.710 mm
V-0
@Thickness 0.0280 in
UL 94 by SABIC-IP
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL 94 by SABIC-IP
Oxygen Index 44 %44 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °FHopper Temperature
Nozzle Temperature 350 - 405 °C662 - 761 °F
Zone 1 340 - 395 °C644 - 743 °F
Zone 2 350 - 405 °C662 - 761 °F
Zone 3 360 - 415 °C680 - 779 °F
Melt Temperature 370 - 410 °C698 - 770 °F
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content 0.020 %0.020 %
 
Descriptive Properties
THERMALPASSESIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 6020 P PES
BASF Ultrason® E 3010 PES
BASF Ultrason® E 1010 PES
3D Systems Fused Deposition Modeling Material ULTEM

PSABI20515 / 213651

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.