MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Dowlex™ 2046G LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: Dowlex™ 2046G Polyethylene Resin is cast extrusion linear low density polyethylene resin grade suitable for artificial turf yarns including slit tapes and monofilaments.
Main Characteristics:
  • Linear Low Density Polyethylene
  • Improved thermal stability for artificial turf yarns, high stiffness monofilament and tape.
Complies with: FDA 21 CRF 177.1520©3.2a. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CRF 177.1520©3.2a

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ASTM D792
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 16.9 MPa2450 psiASTM D882
Film Tensile Strength at Yield, TD 17.6 MPa2550 psiASTM D882
Film Elongation at Break, MD 620 %620 %ASTM D882
Film Elongation at Break, TD 750 %750 %ASTM D882
Elmendorf Tear Strength MD 83 g83 gASTM D1922
Elmendorf Tear Strength TD 290 g290 gASTM D1922
Dart Drop Test 57.0 g0.126 lbASTM D1709A
Film Tensile Strength at Break, MD 59.2 MPa8590 psiASTM D882
Film Tensile Strength at Break, TD 39.9 MPa5790 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °F
Vicat Softening Point 119 °C246 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 2.6 %2.6 %ASTM D1003
Gloss 90 %90 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 274 °C525 °FExtrusion
 
Descriptive Properties
Film Puncture Resistance125 ft-lb/in3
Film Toughness3720 ft-lb/in3TD, ASTM D882
 3910 ft-lb/in3MD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF414 / 311107

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.