Description: Styrene-dissolved, thixotropic, pre-accelerated, orthoophthalic acid based polyester resin. Excellent impregnation features and mechanical characteristics. Application: It is designed for the most critical applications for a thermosetting resin. Resin R 601 is suitable for the production of car parts, shipbuilding, helmets, industrial parts and all other products requiring high resistance. Information provided by Poolkemie |