Description: SAHARA C 070BA is impact copolymer with medium flow viscosity used in injection molding. This grade is characterized by a medium stiffness-impact balance at low temperature as well as a low warpage tendency. The additive formulation provides a good heat aging resistance. This product is typically used in applications that requires high resistance to temperature. This characterized with good heat aging resistance, good impact with low warpage. Product Characteristics: Commercial Status: Active. Processing Method: Injection Molding Typical applications: Battery Cases; Automotive. Information provided by Sahara International Petrochemical Company |