MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® SUPEER™ P8200RT Metallocene Polyethylene (mPE) (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: SABIC® SUPEER™ P8200RT is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. SUPEER™ P8200RT performs well in a wide range of pipe applications with excellent long-term hydrostatic strength, combined with good surface and superior processibility. It is designed to fulfill all the requirements of DIN 16833 / ISO 24033 for PE-RT Type II.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.941 g/ccASTM D792
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 2.3 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60Evaluated using compression molded sample.,Crosshead speed: 500 mm/min.; ASTM D2240
Tensile Strength at Break 35.0 MPaEvaluated using compression molded sample.,Crosshead speed: 500 mm/min.; ASTM D638
Tensile Strength, Yield 20.0 MPaEvaluated using compression molded sample.,Crosshead speed: 500 mm/min.; ASTM D638
Elongation at Break >= 800 %Compression molded sample. Crosshead speed: 500 mm/min.; ASTM D638
Flexural Modulus 650 MPaEvaluated using compression molded sample.,Crosshead speed: 500 mm/min.; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 128 °CEvaluated using compression molded sample.; SABIC method
Vicat Softening Point 121 °CEvaluated using compression molded sample.; ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10207 / 243674

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.