Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes. Compliant with US FDA regulations. Information provided by Zotefoams |