MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Twaron® Aramid Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: Twaron® para-aramid has excellent mechanical properties, chemical resistance, durability, and thermal stability. The characteristics of Twaron® are the result of a 100% paracrystalline structure with molecular chains preferentially oriented along the yarn filament axis.

Twaron® can deliver a range of performance improvements to an exceptionally wide range of high-performance applications, including ballistic protection, heat and chemical protection, and applications for the oil and gas industries. Twaron® is available in black and yellow, and in different types to suit different applications: filament yarn, staple fiber, short-cut fiber, powder, pulp, fabrics and laminates.

Information provided by Teijin Aramid B.V.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.44 - 1.45 g/cc
Moisture Absorption 2.00 - 7.00 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2700 - 3600 MPa
Elongation at Break 2.3 - 4.2 %
Modulus of Elasticity 60.0 - 145 GPa
Tenacity 1.90 - 2.50 N/tex
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °Cstrength retention limit
Minimum Service Temperature, Air -200 °Cmechanical properties retained
Decomposition Temperature 500 °C
Oxygen Index 29 - 40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEIH994 / 287676

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.