MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis BorShape™ FX1001 Polyethylene Film Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: BorShape FX1001 is a blown film grade. It is a high alpha olefin terpolymer polyethylene film grade combining very good extrusion behavior and superior mechanical properties, which are kept in cold conditions BorShape FX1001 has been developed especially for applications requiring high toughness at high stiffness levels.

Applications:

  • Flexible packaging
  • Frozen food packaging
  • Lamination films
  • Heavy-duty bags
  • Medium duty bags
  • Agricultural films
  • Refuse bags
  • Liquid packaging
  • Collation shrink
Additives: BorShape FX1001 contains antioxidant.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.931 g/ccISO 1183
Melt Flow 0.900 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 20.0 g/10 min
@Load 21.0 kg,
Temperature 190 °C
ISO 1133
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %ISO 527-3
Film Elongation at Break, TD 700 %ISO 527-3
Tensile Modulus 350 MPaMD; ISO 527-3
 450 MPaTD; ISO 527-3
Puncture Energy 28.0 JTotal Penetration Energy; ISO 7765-2
Coefficient of Friction, Dynamic 0.400ISO 8295
Tear Strength 60.0 kN/mMD, Elmendorf; ISO 6383/2
 250 kN/mTD, Elmendorf; ISO 6383/2
Dart Drop Test 480 gISO 7765-1
Film Tensile Strength at Break, MD 50.0 MPaISO 527-3
Film Tensile Strength at Break, TD 40.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 127 °CISO 11357-3
 
Optical PropertiesOriginal ValueComments
Haze 80.0 %ASTM D1003
Gloss 7.00 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9671 / 323028

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.