MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Taro Plast Taroblend 45 PC/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC/ABS alloy medium thermal resistance, good flow and mechanical properties. Available: all colors, UV stabilized (L).

Information provided by Taro Plast S.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 - 1.13 g/ccISO 1183
Water Absorption 0.20 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 0.60 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cmISO 2577
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 46.0 MPaISO 527
Elongation at Break 30 %ISO 527
Tensile Modulus 2000 MPaISO 527
Flexural Strength 75.0 MPaISO 178
Flexural Modulus 2150 MPaISO 178
Izod Impact, Notched 450 J/m127x12.7x3.2; ASTM D256
Charpy Impact Unnotched NB80x10x4; ISO 179/1eU
Charpy Impact, Notched 25.0 kJ/m²80x10x4; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Comparative Tracking Index 550 VMethod A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 µm/m-°CISO 11359
Maximum Service Temperature, Air 80.0 °C
@Time 72000 sec
IEC 60216
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75/A
Vicat Softening Point 120 °C
@Load 5.00 kg
ISO 306
 127 °C
@Load 1.00 kg
ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
127x2.17xThickness
Oxygen Index 22 %6.3x12.7x3.2; ASTM D2863
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
60x60xThickness; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTARO096 / 283204

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.