NORYL GTX™ 9400W resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA) that exhibits high heat resistance, high flow, and added mold release. NORYL GTX9400W resin is injection moldable and an excellent candidate for automotive under-the-hood applications such as power distribution boxes, relay boxes, connectors, sensors, and fuse box covers. Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,High Flow,Good Processability Information provided by SABIC |