MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Osterman & Co Osterlene® HD5000-GP HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HD5000-GP is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic properties. Typical applications are rigid food containers such as four, five and six-quart ice cream containers that are produced at high speeds in fast cycling multi-cavity stack molds.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America
Features: Fast Molding Cycle; Good Organoleptic Properties; Good Processability; Good Rigidity; Good Thermal Stability; High Density; High Flow; Low Temperature Impact Resistance; Low Temperature Resistant
Uses: Containers
Processing Method: Injection Molding

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.942 g/ccASTM D792
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D <= 61ASTM D2240
Tensile Strength at Break 3060 psiType IV, 2.0 in.min; ASTM D638
Tensile Strength, Yield 3140 psiType IV, 2.0 in/min; ASTM D638
Elongation at Break 12 %Type IV, 2.0 in.min; ASTM D638
Elongation at Yield 10 %Type IV, 2.0 in.min; ASTM D638
Tensile Modulus 137000 psiYoung's; ASTM D638
Flexural Modulus 137000 psiYoung's; ASTM D790
1% Secant Modulus 100000 psiTensile; ASTM D638
 120000 psiFlexural; ASTM D790
2% Secant Modulus 102000 psiFlexural; ASTM D790
Izod Impact, Notched 0.650 ft-lb/inASTM D256
Izod Impact, Unnotched NBASTM D4812
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 °FPeak; ASTM D3418
Crystallization Temperature 235 °FPeak; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 139 °FUnannealed; ASTM D648
Vicat Softening Point 240 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POSTER039 / 267621

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.