Product Description: Lowinox™ AH25 stabilizer is an excellent performing stabilizer based on sterically hindered dihydroxybenzene CAS No: 79-74-3 EINECS No: 201-222-2 Application: Lowinox™ AH25 stabilizer exhibits excellent protection against oxygen and sun crack. It is recommended for unvulcanized rubber adhesives, tapes and films. Lowinox™ AH25 stabilizer prevents the loss of tack of unvulcanized rubber and reduces the cold flow. Lowinox™ AH25 stabilizer provides good scorch resistance in wire and cable applications. Lowinox™ AH25 stabilizer is effective in a variety of coatings such as unsaturated paint resins where it prevents skinning through oxygen inhibition. Lowinox™ AH25 stabilizer is also particularly useful for stabilizing acrylontrile-based polymers. Information provided by Akrochem Corporation |