MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Agility™ 1021 Performance LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: Agility 1021 Performance LDPE is a high pressure LDPE resin designed to run at faster output rates on blown film lines in LLDPE rich blends while maintaining optics.
Main Characteristics:
  • Faster processing LDPE resin
  • Designed for higher output rates in blends with LLDPE resins at 20-30% loading
  • Optimized molecular structure gives improved optics in blends with LLDPE resins
Complies with: US FDA 21 CFR 177.1520 ©2.2; EU No 10/2011; Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520 ©2.2; EU No 10/2011; Canadian HPFB No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1580 psi
@Thickness 0.0508 mm
ASTM D882
Film Tensile Strength at Yield, TD 1560 psi
@Thickness 0.0508 mm
ASTM D882
Film Elongation at Break, MD 260 %
@Thickness 0.0508 mm
ASTM D882
Film Elongation at Break, TD 540 %
@Thickness 0.0508 mm
ASTM D882
2% Secant Modulus 24400 psi
@Thickness 0.0508 mm
MD; ASTM D882
 26800 psi
@Thickness 0.0508 mm
TD; ASTM D882
Elmendorf Tear Strength MD 460 g0.002; ASTM D1922
Elmendorf Tear Strength TD 250 g0.002; ASTM D1922
Dart Drop Test 100 g
@Thickness 0.0508 mm
ASTM D1709A
Film Tensile Strength at Break, MD 3130 psi
@Thickness 0.0508 mm
ASTM D882
Film Tensile Strength at Break, TD 2380 psi
@Thickness 0.0508 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 226 °F
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %
@Thickness 0.0508 mm
ASTM D1003
Gloss 60 %
@Thickness 0.0508 mm
45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 404 °FExtrusion
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance58.9 ft-lb/in32.0 mil
Film Toughness553 ft-lb/in3MD, ASTM D882
 727 ft-lb/in3TD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF386 / 311079

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.